| Formula | Ce3+:Y3Al5O12 |
| Crystal structure | cubic |
| Melting point | 1950 oC |
| Density | 4.55g/cm3 |
| Hardness | 8.5 Mohs |
| Index of refraction | 1.82 |
| Decay constants | 70ns |
| Doping concentration | 1% |
![]() |
![]() |
| Home | Products | Design Service | Contact Us |
|
Green Laser Microchip,
Nd:YVO4,
Nd:GdVO4,
Nd:YAG,
Yb:YAG,
Cr4+:YAG,
Ce3+:YAG, Nd3+:Ce3+:YAG, Er3+:YAG, Mg:Cr:LiTaO3, Ti3+:Al2O3, Laser Ruby Cerium Doped Yttrium Aluminum Garnet (Ce3+: YAG)
Cerium Doped Yttrium Aluminum Garnet (Ce3+: YAG) is a kind of scintillator material that is often used to convert high energy electrons to visible light of 550nm. Typically, Ce3+: YAG can be used in scanning electron microscopes (SEM) for detecting back scattered electrons, in the transmission electron microscopes (TEM) for high resolution digital imaging, or in the electron energy loss spectrometer (EELS). We offer high quality Ce3+: YAG with different specifications and dimensions for use in the fields of electron microscopy and analytical electron microscopy. Main Specifications:
Contact Us
Sales Office in Shanghai
Live Chat
Tel: 86-21-58325141 Fax: 86-21-58329412 E-mail: sales@pantotek.com |
Copyright 2004 - 2006 Pantotek Technologies Inc., All Rights Reserved.
Tel: (86) 021-58325141, Fax: (86) 021-58329412